Just for your information guys, about "cheap" chinese diving lights. Have two of them, one is okay and one looks like this now after 3rd dive. Any recommendations for new chinese lights? Cause never Brynite again

Welcome to ScubaBoard, the world's largest scuba diving community. Registration is not required to read the forums, but we encourage you to join. Joining has its benefits and enables you to participate in the discussions.
Benefits of registering include